Liquid silicone over glass molds: glass insert fixing, clear mark-free encapsulation and optical surface protection, solving bubbles

Liquid Silicone Over Glass

Precision encapsulation of LSR over glass is used for camera windows, AR/VR optics and medical ultrasound windows. The difficulties: glass is fragile, the optical surface must not be scratched, and bubbles and stress marks must be avoided.

Mold Design Highlights

  • Glass insert fixing: flexible locating plus vacuum suction to hold the glass and avoid clamping stress and chipping;
  • Mirror cavity: polish the area opposite the optical active surface to mirror level to protect the glass finish;
  • Mark-free parting: keep the parting line away from the optical active area, in a non-visible or hidden position;
  • Low-stress filling: balanced, slow gating to reduce weld lines and optical distortion from internal stress;
  • Venting: vent fully at ends and high points or use vacuum to eliminate bubbles in the encapsulation layer.

Process Recommendation

Mold temperature 170~195C; control filling speed and holding pressure; over-curing can slightly yellow the silicone and reduce transmission. Use transmittance and haze as outgoing criteria.

Common Defects

  • Bubbles in the layer: insufficient venting;
  • Optical distortion: internal stress or flow marks;
  • Glass chipping: improper locating or ejection stress.

Delivery

Structure design, insert locating solution and trial validation of glass overmolding molds, with optical and air-tightness testing advice.